The Florida Department of Transportation (FDOT) conducted an experiment to address the effects of polymer modifiers on the performance of Superpave® mixes by using a heavy vehicle simulator. Two fine-graded Superpave mixes were considered. One mix included a virgin binder meeting the requirements of PG 67-22, and the other contained a styrene– butadiene–styrene polymer (SBS)-modified binder meeting those of PG 76-22. Both respective mixes contained the same effective binder content, aggregate components, and gradation. The mixes were designed for 10 million to 30 million equivalent single-axle loads with the use of the standard Superpave mix design methodology. During placement of these mixes, all standard FDOT density requirements and acceptance criteria were applicable. The subsequent investigation showed that the sections with SBS-modified mixture significantly outperformed those with the unmodified mixture. It was also determined that rutting in the unmodified mixture was primarily a function of shear flow, whereas rutting in the SBS-modified mixture was caused mainly by densification. This paper presents a description of the testing program, the data collection effort, and the subsequent analyses and findings, focusing primarily on the initiation mechanisms of rutting in asphalt mixtures as generated and observed under accelerated pavement testing.
Rut Initiation Mechanisms in Asphalt Mixtures as Generated under Accelerated Pavement Testing
Transportation Research Record
Transportation Research Record: Journal of the Transportation Research Board ; 1940 , 1 ; 136-145
2005-01-01
Article (Journal)
Electronic Resource
English
Rut Initiation Mechanisms in Asphalt Mixtures as Generated Under Accelerated Pavement Testing
Transportation Research Record | 2005
|Accelerated Pavement Testing of Re-Recycled Cold Central Plant Recycled Asphalt Mixtures
Transportation Research Record | 2024
|