TO MAKE DOCUMENT CONSISTENT WITH AS81820/1-4 AND AS81820, REMOVING CHROME PLATING AS AN OPTION. REMOVING AMS2700, METHOD 1, TYPE 8 PASSIVATION AS AN OPTION IN THE FUTURE.
BEARING, PLAIN, SELF-LUBRICATING, SELF-ALIGNING, LOW SPEED, NARROW, CHAMFERED RACE, -65 TO +325 °F
2018-05-14
Conference paper
English
BEARING, PLAIN, SELF-LUBRICATING, SELF-ALIGNING, LOW SPEED, NARROW, CHAMFERED RACE, -65 TO +325 °F
SAE Technical Papers | 2008
BEARING, PLAIN, SELF-LUBRICATING, SELF-ALIGNING, LOW SPEED, NARROW, CHAMFERED RACE, -65 TO 325 °F
SAE Technical Papers | 2004
BEARING, PLAIN, SELF-LUBRICATING, SELF-ALIGNING, LOW SPEED, NARROW, CHAMFERED RACE, -65 TO 325 °F
SAE Technical Papers | 2003
BEARING, PLAIN, SELF-LUBRICATING, SELF-ALIGNING, LOW SPEED, NARROW, CHAMFERED RACE, −65 TO +325 °F
SAE Technical Papers | 2010
SAE Technical Papers | 2014