This SAE Standard covers the mechanical and physical property requirements for Austempered Ductile Iron (ADI) castings used in automotive and allied industries. Specifically covered are: a Hardness b Tensile Strength c Yield Strength d Elongation e Modulus of Elasticity f Impact Energy g Microstructure In this document SI units are primary and in-lb units are derived. Appendix A provides general information and related resources on the microstructural, chemical and heat treatment requirements to meet the mechanical properties needed for ADI in particular service conditions and applications.
Automotive Austempered Ductile (Nodular) Iron Castings (ADI)
2004-05-26
Conference paper
English
Impact tests , Test procedures , Iron , Heat treatment , Casting , Steel , Identification , Suppliers , Tensile strength
Automotive Austempered Ductile (Nodular) Iron Castings (ADI)
SAE Technical Papers | 2018
Automotive Austempered Ductile (Nodular) Iron Castings (ADI)
SAE Technical Papers | 2003
AUTOMOTIVE DUCTILE (NODULAR) IRON CASTINGS
SAE Technical Papers | 1986
Automotive Ductile (Nodular) Iron Castings
SAE Technical Papers | 2017
Automotive Ductile (Nodular) Iron Castings
SAE Technical Papers | 2004