Selectively densified rollers from Distaloy DC-1, Astaloy Mo and Distaloy AE have been rolling contact fatigue (RCF) tested on a ZF-test rig. The rolling contact fatigue endurance limit of the Astaloy Mo based material is approximately 1500 MPa that can be compared to the selected reference material, AISI 5115 (DIN 16MnCr5), 1600 MPa. For the diffusion-alloyed materials, Distaloy DC1 and Distaloy AE, it was not possible to determine the endurance limit due to too few tests. However, the endurance limit seems to be slightly lower than the Astaloy Mo material. The case depth seems to be low for all materials, but the effect appears to be more severe for the Distaloy DC1 material. Surface cracks of different character could be found in all specimens. Small cracks associated with smaller pits are found on the run outs (>50·106 cycles).


    Access

    Check access

    Check availability in my library

    Order at Subito €


    Export, share and cite



    Title :

    Rolling Contact Fatigue Tests of Selectively Densified Materials


    Additional title:

    Sae Technical Papers


    Contributors:

    Conference:

    Automotive and Transportation Technology Congress and Exposition ; 2001



    Publication date :

    2001-10-01




    Type of media :

    Conference paper


    Type of material :

    Print


    Language :

    English


    Keywords :


    Rolling contact fatigue tests of selectively densified materials

    Bengtsson,S. / Forden,L. / Johansson,P. et al. | Automotive engineering | 2001


    2001-01-3285 Rolling Contact Fatigue Tests of Selectively Densified Materials

    Bengtsson, S. / Forden, L. / Johansson, P. et al. | British Library Conference Proceedings | 2001



    Evaluating the rolling contact fatigue properties of surface densified PM gears

    Lawcock,R. / Stackpole,US | Automotive engineering | 2006


    Controlling rolling contact fatigue

    Transport Writing Services Ltd. Postfach PO Box 274 GB - TN1 2ZL Tunbridge Wells, Kent | IuD Bahn | 2002