When the alkali metal-supported catalyst was treated at 830°C, the NOx conversion decreased because the alkali metals in the catalyst layer gradually moved to the cordierite honeycomb layer and reacted with the cordierite elements. This phenomena decreased to be added the basic metal oxide (α) in the catalyst layer. The improved catalyst with α 2 showed higher performance than the conventional catalyst in the model gas test. Moreover, the emission values of NOx, HC, and CO were 50% or less than Japanese domestic regulation values even after 830°C×60h heat treatment in a vehicle test.
Improvement of Heat Resistance for Lean NOx Catalyst
Sae Technical Papers
SAE 2004 World Congress & Exhibition ; 2004
2004-03-08
Conference paper
English
Improvement of Heat Resistance for Lean N0x Catalyst
British Library Conference Proceedings | 2004
|Improvement of heat resistance for the lean NOx catalyst
Automotive engineering | 2004
|2004-01-1495 Improvement of Heat Resistance for Lean NOx Catalyst
British Library Conference Proceedings | 2004
|Improvement of SOx Durability and Heat Resistance for Lean NOx Catalyst
SAE Technical Papers | 2002
|Improvement of SOx durability and heat resistance for lean NOx catalyst
Automotive engineering | 2002
|