By suitable control of thermal conditions in directional-solidification process, supperalloy structural and machine components (e.g., turbine blades) cast with microstructures enhancing resistance to fatigue. Specific version of process and thermal conditions chosen to reduce micro-segregation during solidification and to minimize or eliminate script carbide and eutectic-phase inclusions, which are brittle inclusions found to decrease resistance to fatigue.
Eutectic-Free Superalloy Made By Directional Solidification