Reducing convection during plane-front, two-phase peritectic solidification reduces banding. Experiments show reducing radial thermal gradients and flattening solidification interface reduces compositional banding associated with plane-front, two-phase peritectic solidification. Possibility of coupled two-phase peritectic composite solidification still exists. Previously thought banding was inevitable.


    Access

    Access via TIB

    Check availability in my library


    Export, share and cite



    Title :

    Progress Toward Monolithic Peritectic Solidification


    Contributors:

    Published in:

    Publication date :

    1987-02-01



    Type of media :

    Miscellaneous


    Type of material :

    No indication


    Language :

    English


    Keywords :



    Peritectic Solidification of Highly Undercooled Cu-Co Alloy

    Cao, C. D. / Lu, X. Y. / Wei, B. et al. | British Library Conference Proceedings | 1999



    Microstructure Evolution of Ti-Al Peritectic System during the Initiated Stage of Directional Solidification

    Su, Y. Q. / Liu, C. / Li, X. Z. et al. | British Library Conference Proceedings | 2007


    Growth of Metastable Peritectic Alloys

    Larson, David J., Jr. / Pirich, Ronald G. | NTRS | 1987