Cooling at certain rates produced fibrous composite structures. Alloy samples melted in alumina or graphite crucibles under argon and then chillcast into 33-mm-diameter rods or sucked directly into 3-mm-bore alumina or silica tubes. Alloying not automatic with immiscible components of different densities and widely different melting points.
Directional Solidification of Monotectic Alloys
NASA Tech Briefs ; 7 , 4
1983-10-01
Miscellaneous
No indication
English
Directional Solidification Of Monotectic Alloys