In this work we report the structural, optical and electrical properties of CdS thin films prepared by chemical bath deposition (CBD) under the effect of solution temperatures. The solution temperatures used vary between 55 and 75 °C. The XRD patterns show that the films have a hexagonal phase with a preferential (002) orientation. The structural parameters such as the grain size, dislocation density and strain are calculated. The transmission spectra, recorded in the UV visible range, reveal a high transmission coefficient (85%) of the prepared films and an optical band gap values of 2 – 2.4 eV. The electrical measurements show that the dark conductivity values increase from 10−7 to 10−4 (Ω.cm)−1 at higher temperature (Ts > 65°C). It is found that the photoconductivity of the deposited films is two to five decades larger than the dark conductivity, and the photoconductivity to the dark conductivity ratio obtained at 3000 Lx vary from 102 to 105. From these results we inferred that the elaborated CdS thin films exhibit good properties intended for solar cell window layers.


    Access

    Check access

    Check availability in my library

    Order at Subito €


    Export, share and cite



    Title :

    Preparation and characterization of CdS thin films


    Contributors:
    Moualkia, H. (author) / Attaf, N. (author) / Hadjeris, L. (author) / Herissi, L. (author) / Abdelmalek, N. (author)


    Publication date :

    2012-03-01


    Size :

    651225 byte




    Type of media :

    Conference paper


    Type of material :

    Electronic Resource


    Language :

    English



    Preparation and characterization of RuO2 thin films

    Huang, Y.S. | Online Contents | 1999


    Sulfated Glycopolymer Thin Films-Preparation, Characterization, and Biological Activity

    Grombe, R. / Gouzy, M. F. / Maitz, M. F. et al. | British Library Online Contents | 2007