A method for producing a motor vehicle component is disclosed having the steps of providing a strain-hardened blank composed of a 5000 grade aluminum alloy, partially heating the blank in a first region to a temperature higher than 350° C., in particular higher than 400° C., and in a second region to a temperature between 150° C. and 350° C., preferably to 300° C., in less than 20 s, preferably less than 10 s and in particular in 2 to 5 s, and transferring the blank into a cooling tool, and performing cooling in less than 20 s, preferably less than 10 s and in particular in 2 to 5 s.
Method for producing a motor vehicle component from aluminum
2017-11-21
Patent
Electronic Resource
English
IPC: | C22F CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS OR NON-FERROUS ALLOYS , Verändern der physikalischen Struktur von Nichteisenmetallen oder Nichteisenlegierungen / B21D WORKING OR PROCESSING OF SHEET METAL OR METAL TUBES, RODS OR PROFILES WITHOUT ESSENTIALLY REMOVING MATERIAL , Bearbeiten oder Verarbeiten von Blechen, Metallrohren, -stangen oder -profilen ohne wesentliches Abtragen des Werkstoffs / B62D MOTOR VEHICLES , Motorfahrzeuge / C21D Veränderung der physikalischen Struktur von Eisenmetallen , MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS / C22C Legierungen , ALLOYS |
Method for producing a motor vehicle component from aluminum
European Patent Office | 2018
|Method for producing a motor vehicle component from aluminum
European Patent Office | 2018
|METHOD FOR PRODUCING A MOTOR VEHICLE COMPONENT FROM ALUMINUM
European Patent Office | 2015
|METHOD FOR PRODUCING A MOTOR VEHICLE COMPONENT FROM ALUMINUM
European Patent Office | 2015
|METHOD FOR PRODUCING A MOTOR VEHICLE COMPONENT FROM ALUMINUM
European Patent Office | 2015
|