Sulfur-crosslinkable rubber mixture (I) comprises: at least a functionalized diene rubber, whose functionalization is present along the polymer chain and/or at the end and enables for binding at fillers, where the diene rubber has a glass transition temperature of -110 to -15[deg] C; at least an aliphatic and/or aromatic hydrocarbon resin with a softening point (ring and ball according to ASTM E 28) of 50-150[deg] C and a number average molecular weight of 200-2000 g/mole and a polydispersity of 15; and at least a filler.