Investigation of corrugation of various types of rails; high and low spots give corrugated appearance to surface; depth is about 2 mm., wavelength is 35 to 60 mm.; physical properties and microphotographs. (See also - discussion p 54-59)
Supplementary researches on undulatory wear resistance of rail steels
Recherches complementaires sur la resistance a l'usure ondulatoire des aciers a rails
1930
15 pages
39 Figs. Partly on Supp. plates
Article (Journal)
French
© Metadata Copyright Elsevier B. V. All rights reserved.