To analyze the relationship between composition, microstructure and mechanical properties of TA15 titanium alloys, the quasi-static tensile properties and dynamic properties at room temperature of four kinds of TA15 titanium alloys were studied by the electronic universal tensile testing machine and split hopkinson pressure bar (SHPB). The results reveal that the Zr content has little effect on the tensile strength at room temperature, moreover, with the increase of content of main alloy elements Al, V and Mo, the content of primary α phase decreases and the lamella width of secondary α phase is thinner which provide higher strength and lower plasticity. Slight changes in alloy composition have little effect on dynamic mechanical properties within the critical strain rate range. Increasing the content of main alloy elements Al, Zr, V and Mo is beneficial to improve the critical strain rate, at which the alloy has excellent dynamic mechanical properties. For equiaxed TA15 titanium alloys obtained under air cooling condition, the smaller volume fraction of primary α phase and thinner lamella of secondary α phase can improve the tensile strength, critical strain rate and dynamic mechanical properties at room temperature.
Effect of composition on microstructure and mechanical properties of TA15 titanium alloy
2019
Article (Journal)
Electronic Resource
Unknown
Metadata by DOAJ is licensed under CC BY-SA 1.0
Influence of laser shock peening times on microstructure and hardness of TA15 titanium alloy
British Library Online Contents | 2014
|Microstructure and Mechanical Properties of Laser Melting Deposited TA15+Ti2AlNb Alloys
DOAJ | 2017
|Study on the fatigue properties of the TA15 titanium alloy plate and electron beam welding specimen
British Library Online Contents | 2003
|Effect of oxygen content on microstructure and mechanical properties of ZTA15 titanium alloy
DOAJ | 2025
|