In a process for producing a cold- or hot-rolled steel strip from an ultrahigh-strength multiphase steel having a particular composition the required multiphase microstructure is generated during continuous heat treatment. The cold- or hot-rolled steel strip is heated in the continuous heat treatment furnace to a temperature in the range from 700 to 950° C. and the heat-treated steel strip is subsequently cooled from the heat treatment temperature at a cooling rate of from 15 to 100° C./s to a first intermediate temperature of from 300 to 500° C. followed by cooling at a cooling rate of from 15 to 100° C./s to a second intermediate temperature of from 200 to 250° C.; the steel strip is subsequently cooled at a cooling rate of from 2 to 30° C./s in air to room temperature or the cooling at a cooling rate of from 15 to 100° C./s is maintained from the first intermediate temperature to room temperature.


    Access

    Download


    Export, share and cite



    Title :

    Ultrahigh-strength multiphase steel with improved properties during production and processing


    Contributors:

    Publication date :

    2019-04-30


    Type of media :

    Patent


    Type of material :

    Electronic Resource


    Language :

    English


    Classification :

    IPC:    C21D Veränderung der physikalischen Struktur von Eisenmetallen , MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS / B62D MOTOR VEHICLES , Motorfahrzeuge / C22C Legierungen , ALLOYS



    ULTRAHIGH-STRENGTH MULTIPHASE STEEL HAVING IMPROVED PROPERTIES DURING PRODUCTION AND PROCESSING

    SCHULZ THOMAS / WEDEMEIER ANDREAS / SPROCK WILFRIED et al. | European Patent Office | 2019

    Free access


    Properties of direct-quenched aircraft forged component made of ultrahigh-strength steel 300M