By differential scanning calorimetry method have been studied influence of nanotubes upon structure mechanism of gelation of composition. It is shown that particles of carbonanotube are active nucleation agents for crystallization of polipropilen. Crystallization takes place on the mechanism of the strained matrix. After by the got results, at content of carbonanotube of 1-2 % there are the best terms for crystallization of polymeric matrix
Application of method of differential scanning calorimetry is for the study of mechanism of gelation of composition on the basis of carbonanotube
2013
Article (Journal)
Electronic Resource
Unknown
Metadata by DOAJ is licensed under CC BY-SA 1.0
Differential Scanning Calorimetry
TIB AV-Portal | 2022
|Differential Scanning Calorimetry Study of Asphalt Crystallinity
Online Contents | 1996
|Differential Scanning Calorimetry Study of Asphalt Crystallinity
Transportation Research Record | 1996
|Differential Scanning Calorimetry Study of Asphalt Crystallinity
Transportation Research Record | 1996
|Evaluation of Automotive Crankcase Lubricants by Differential Scanning Calorimetry
SAE Technical Papers | 1982
|