Stress corrosion cracking (SCC) and hydrogen embrittlement (HE) of pipeline steels in contact with soil was investigated. Different soils were prepared in order to determine their physical, chemical and bacteriological characteristics. Slow strain rate testing was carried out by using aqueous extracts from soil samples and NS4 standard solution. Stress vs. strain curves of API 5L grade X46 steel were obtained at different electrode potentials (Ecorr, 100 mV below Ecorr and 300 mV below Ecorr) with 9 × 10−6 s−1 and 9 × 10−7 s−1 strain rate. In addition, the hydrogen permeation tests were carried out in order to evaluate the susceptibility of hydrogen penetrates into theses steels. The results demonstrated the incidence of cracking and their dependence on the potential imposed. In that case, cracking occurred by stress corrosion cracking (SCC) and the hydrogen embrittlement (HE) had an important contribution to cracking initiation and propagation. Cracking morphology was similar to the SCC reported on field condition where transgranular cracking were detected in a pipeline collapsed by land creeping. It was important to point out that even under cathodic potentials the material showed the incidence of secondary cracking and a significant reduction of ductility.
Evaluation of stress corrosion cracking and hydrogen embrittlement in an API grade steel
Engineering Failure Analysis ; 36 ; 423-431
2014
9 Seiten, 18 Quellen
Aufsatz (Zeitschrift)
Englisch
Hydrogen Embrittlement and Stress Corrosion Cracking of Titanium Alloys Caused by Cleaning Processes
SAE Technical Papers | 1985
|