Full scale laboratory studies using curved laminated safety glass windshields, a horizontal accelerator, and a 50th percentile dummy to provide impact performance are presented. Lacerative damage based on moist chamois face covering and Severity Indices for annealed glass windshield configurations were obtained on the current domestic automobile windshield, experimental thin annealed glass windshields in symmetrical and asymmetrical glass configurations, and windshields with 0.045 in. HPR interlayer.Symmetrical thin glass windshields, such as, 0.050 in glass, gave excellent performance to 38 mph. Lacerative damage decreases as the inboard glass thickness decreases for windshields having 0.030 in. HPR interlayer and 1/8 in. float glass outboard ply. Windshields with 0.045 in. HPR interlayer, designed to improve penetration resistance, have somewhat higher Severity Indices. Such windshields will require further study.


    Zugriff

    Zugriff prüfen

    Verfügbarkeit in meiner Bibliothek prüfen

    Bestellung bei Subito €


    Exportieren, teilen und zitieren



    Titel :

    Safety Performance of Laminated Glass Structures


    Weitere Titelangaben:

    Sae Technical Papers


    Beteiligte:
    Chabal, J. (Autor:in) / Rieser, R. G. (Autor:in)

    Kongress:

    Mid-Year Meeting ; 1970



    Erscheinungsdatum :

    01.02.1970




    Medientyp :

    Aufsatz (Konferenz)


    Format :

    Print


    Sprache :

    Englisch




    Safety Performance of Laminated Glass Configurations

    Chabal, J. / Rieser, R. G. | SAE Technical Papers | 1967


    LAMINATED SAFETY GLASS

    CLOOTS TOM / LOCCUFIER JOHAN / FRANSEN GUIDO | Europäisches Patentamt | 2020

    Freier Zugriff

    Laminated safety glass

    CLOOTS TOM / LOCCUFIER JOHAN / FRANSEN GUIDO | Europäisches Patentamt | 2020

    Freier Zugriff

    Laminated Safety Glass

    McCarroll, R. H. | SAE Technical Papers | 1937


    Laminated safety glass

    McCarroll, R.H. | Engineering Index Backfile | 1937