This specification covers one grade of commercially pure titanium in the form of seamless tubing. AMS4942H results from a Five-Year Review and update of this specification with changes to revise the annealing practice to historical temperatures based on grain growth and property changes resulting from higher annealing temperatures previously indicated (3.3), update language related to unauthorized exceptions (3.7, 4.4.1, 5.1.1, 8.4), add ASTM E539 analytical method (2.2, 3.1), update applicable documents (Section 2), and allow use of immediate prior specification revision (8.5).
Titanium Tubing, Seamless Annealed, 40.0 ksi (275 MPa) Yield Strength
2022-07-08
Aufsatz (Konferenz)
Englisch
Titanium Tubing, Seamless Annealed, 40.0 ksi (275 MPa) Yield Strength
SAE Technical Papers | 2018
Titanium Tubing, Seamless Annealed, 40.0 ksi (275 MPa) Yield Strength
SAE Technical Papers | 2006
Titanium Tubing, Seamless Annealed, 40.0 ksi (275 MPa) Yield Strength
SAE Technical Papers | 2010
TITANIUM TUBING, SEAMLESS Annealed, 40,000 psi, Yield
SAE Technical Papers | 1964
TITANIUM TUBING, SEAMLESS Annealed, 40,000 psi (276 MPa) Yield Strength
SAE Technical Papers | 1977