The tensile and shear properties of eight soft solders were determined at several loading rates at 78, −100, −320, and −423 F. In general it was found that the tensile and shear strengths increased with increase in loading rate and decrease in temperature. Large decreases in ductility, as measured by elongation and reduction in area, and decreased tensile and shear strengths for some of the solders at cryogenic temperatures are indicative of their low temperature embrittlement. A discussion of the experimental data and literature values is given and recommendations are made concerning the application of solders for cryogenic service.


    Zugriff

    Zugriff prüfen

    Verfügbarkeit in meiner Bibliothek prüfen

    Bestellung bei Subito €


    Exportieren, teilen und zitieren



    Titel :

    Tensile and Shear Properties of Several Solders at Cryogenic Temperatures


    Weitere Titelangaben:

    Sae Technical Papers


    Beteiligte:
    Watson, J. F. (Autor:in) / Christian, J. L. (Autor:in)

    Kongress:

    Pre-1964 SAE Technical Papers ; 1906



    Erscheinungsdatum :

    01.01.1962




    Medientyp :

    Aufsatz (Konferenz)


    Format :

    Print


    Sprache :

    Englisch




    Study of Tensile Properties of Mg-Rare Earth Alloys at Cryogenic Temperatures

    Wang, Hao / Dong, Shangli / Lu, Gang | Springer Verlag | 2012



    Cryogenic Tensile Properties of Selected Aerospace Materials

    W. Weleff / W. F. Emmons / H. S. McQueen | NTIS | 1964


    Cryogenic Tensile Properties of Selected Aerospace Materials

    W. Weleff / W. F. Emmons / H. S. McQueen | NTIS | 1964


    Solders

    SAE Technical Papers | 2018