Special fixture holds specimen of laminated composite material in 20-klb (89-kN) or larger load frame for compression-after-impact test. In preparation for test, specimen damaged by dropping weight on it at known kinetic energy. During test, specimen loaded in compression, and load measured, until specimen fails. Measurement data used to characterize compressive strength of specimen after impact important indicator of ability of structural components made of composite material to tolerate damage. Tests give more-realistic measures of tolerance to damage.


    Zugriff

    Zugriff über TIB

    Verfügbarkeit in meiner Bibliothek prüfen


    Exportieren, teilen und zitieren



    Titel :

    Fixture For Compression-After-Impact Tests Of Thin Specimens


    Beteiligte:

    Erschienen in:

    Erscheinungsdatum :

    1994-04-01



    Medientyp :

    Sonstige


    Format :

    Keine Angabe


    Sprache :

    Englisch


    Schlagwörter :



    Width Effects on Compression Strength of Composite Sandwich Test Specimens After Barely Visible Impact Damage

    Vizzini, A. / Harris, J. / Moody, R. | British Library Conference Proceedings | 1999


    Characteristics of Charpy impact tests using C-notch specimens

    Saruki, K. / Yamada, A. / Aoyama, S. | Tema Archiv | 1984