Toughness increased without sacrificing processability or hot strength. Resin composition provides best overall balance of composite toughness and retention of mechanical properties at 600 degree F (316 degree C) with processability obtained by substituting 20 mole percent of diamine used in PMR-15 resins with diamine containing twice number of flexible phenyl connecting groups.
PMR Composites Of Increased Toughness