Ground-based research on the containerless melting of glass and experiments performed during a flight on the SPAR 6 are described. Experiments leading to selection of the flight sample composition, a silica-modified gallia/calcia glass, and the preparation of a one quarter inch diameter flight sample are described. During the flight experiment, a sample of the glass was containerless melted and cooled to a clear glass in a single axis acoustic positioning apparatus. The functioning of the flight experimental hardware was evaluated. The evaluation of the sample is presented.