Metals and fluoropolymers exposed to 0.5 to 1.0 keV argon ions at current densities of 0.2 to 1.5 mA/sq cm develop surface texturing that increases tensile and shear strength of epoxy bonds. Bonds are 46 to 100 percent stronger than those of chemically etched surfaces. Metals require 3 to 4 hours of bombardment to become properly textured. Fluoropolymers require 5 seconds to 30 minutes. Ion beam will not texture nickel. Unlike chemical treatments, bonding of fluoropolymers can be done days or months after ion treatment.


    Zugriff

    Zugriff über TIB

    Verfügbarkeit in meiner Bibliothek prüfen


    Exportieren, teilen und zitieren



    Titel :

    Ion-beam etching enhances adhesive bonding


    Beteiligte:
    Banks, B. A. (Autor:in) / Mirtich, M. J. (Autor:in) / Sovey, J. S. (Autor:in)

    Erschienen in:

    Erscheinungsdatum :

    1980-08-01



    Medientyp :

    Sonstige


    Format :

    Keine Angabe


    Sprache :

    Englisch


    Schlagwörter :


    Bush for stabilizer, adhesive bonding tool, and adhesive bonding method

    KURODA SHIGERU / OMURA SHUJI | Europäisches Patentamt | 2015

    Freier Zugriff



    Adhesive Bonding of Aluminium

    Bjorgum, A. / Nordlien, J. H. / Lunder, O. R. et al. | SAE Technical Papers | 2001


    Adhesive bonding flies high

    Alanson, R.M. | Tema Archiv | 1997