Resistance measurements showing that vitreous graphite remains almost wholly intact even after 1 hour of contact with silicon melt indicates that vitreous carbon may be superior to rubbed-on graphite as interface between ceramic substrate and silicon layer of solar cell.


    Zugriff

    Zugriff über TIB

    Verfügbarkeit in meiner Bibliothek prüfen


    Exportieren, teilen und zitieren



    Titel :

    Improved silicon/carbon interface for solar cells


    Beteiligte:
    Zook, D. J. (Autor:in)

    Erschienen in:

    Erscheinungsdatum :

    1979-12-01



    Medientyp :

    Sonstige


    Format :

    Keine Angabe


    Sprache :

    Englisch