Control of porosity in weld beads was major objective in development of aluminum welding program. Porosity, most difficult defect to control, is caused by hydrogen gas unable to escape during solidification. Hard tooling allows hotter bead than free-fall tooling so hydrogen bubbles can boil out instead of forming pores. Welding position, moisture, and cleanliness are other important factors in control of porosity.


    Zugriff

    Zugriff über TIB

    Verfügbarkeit in meiner Bibliothek prüfen


    Exportieren, teilen und zitieren



    Titel :

    Technology of welding aluminum alloys-III


    Beteiligte:
    Harrison, J. R. (Autor:in) / Kor, L. J. (Autor:in) / Oleksiak, C. E. (Autor:in)

    Erschienen in:

    Erscheinungsdatum :

    01.03.1978



    Medientyp :

    Sonstige


    Format :

    Keine Angabe


    Sprache :

    Englisch


    Schlagwörter :


    Technology of welding aluminum alloys-I

    Harrison, J. R. / Korb, L. J. / Oleksiak, C. E. | NTRS | 1978



    Technology of welding aluminum alloys-IV

    Ginez, R. / Lewis, J. R. / Millett, A. U. et al. | NTRS | 1978


    Resistance welding of aluminum alloys

    Fassler, P.W. | Engineering Index Backfile | 1937