The present disclosure provides Al—Si—Mg aluminum alloys comprising a deliberate addition of Mn between 0.05-0.40 weight percent to increase at least one tensile property (such as the yield strength) of an aluminum product comprising such alloy. The Al—Si—Mg alloy comprises, in weight percent, 5-9% Si, 0.35-0.75% Mg, 0.05-0.4% Mn, less than 0.15% Fe, up to 0.15% Ti, 0.005-0.03% Sr and the balance being aluminum and unavoidable impurities, wherein the unavoidable impurities may be present in an amount of up to 0.05% each and up to 0.15% total. The present disclosure provides a foundry ingot comprising the above Al—Si—Mg aluminum alloy, a process for making the above Al—Si—Mg aluminum alloy and an aluminum alloy obtainable by said process.
Aluminum alloys having improved tensile properties
14.12.2021
Patent
Elektronische Ressource
Englisch
Room Temperature and 600F Tensile Properties of Aluminum-Silicon Casting Alloys
SAE Technical Papers | 1968
|Tensile, fatigue, and creep properties of forged aluminum alloys at temperatures up to 800 F
Engineering Index Backfile | 1948
|Aluminum material having improved precipitation hardening
Europäisches Patentamt | 2018
|