PROBLEM TO BE SOLVED: To provide a tire vulcanization mold capable of preventing poor appearance of a tire, a manufacturing method of a pneumatic tire using the same and the pneumatic tire.SOLUTION: There is provided a vulcanization mold 1 for molding a pneumatic tire having a tread part 3 and a side wall part 4. It contains a tread segment 6 and a side wall mold 7 and the tread segment 6 and the side wall part 7 are arranged with capability of contacting and releasing and a tread molded face 6a and a side wall molded face 7s are continued with a split surface 9 by contacting each other during mold fastening when tire vulcanization. At least one of the tread molded face 6s or the side wall molded face 7s contains a first projecting stripe part 10 extruding in a tire side at a position neighboring the split surface 9. The first projecting stripe part 10 is formed from a plurality of first projection 12 extending along a tire circumferential direction via a first gap 11.SELECTED DRAWING: Figure 2
【課題】タイヤの外観不良を抑制しうるタイヤ加硫金型、それを用いた空気入りタイヤの製造方法、及び、空気入りタイヤに関する。【解決手段】トレッド部3とサイドウォール部4とを有する空気入りタイヤを成形するための加硫金型1である。トレッドセグメント6とサイドウォール型7とを含み、トレッドセグメント6とサイドウォール型7とは、接離可能に配されるとともに、タイヤ加硫時の型締時に互いに接触してトレッド成形面6sとサイドウォール成形面7sとを割面9で連続させる。トレッド成形面6s又はサイドウォール成形面7sの少なくとも一方は、割面9に隣接した位置でタイヤ側に突出する第1凸条部10を含む。第1凸条部10は、第1隙間11を介してタイヤ周方向に沿ってのびる複数の第1突起12から形成されている。【選択図】図2
TIRE VULCANIZATION MOLD, MANUFACTURING METHOD OF PNEUMATIC TIRE USING THE SAME AND PNEUMATIC TIRE
タイヤ加硫金型、それを用いた空気入りタイヤの製造方法、及び、空気入りタイヤ
01.12.2016
Patent
Elektronische Ressource
Japanisch
PNEUMATIC TIRE, TIRE VULCANIZATION MOLD, AND METHOD OF MANUFACTURING PNEUMATIC TIRE
Europäisches Patentamt | 2020
|PNEUMATIC TIRE, TIRE VULCANIZATION MOLD AND METHOD FOR MANUFACTURING PNEUMATIC TIRE
Europäisches Patentamt | 2021
|PNEUMATIC TIRE, MOLD FOR TIRE VULCANIZATION AND MANUFACTURING METHOD FOR PNEUMATIC TIRE
Europäisches Patentamt | 2016
|