Welded joints of airframes critical to the flight-safety are commonly repair welded during its operational live. In this study, the effect of up to three weld repairs by gas tungsten arc welding (GTAW) on the axial fatigue strength of AISI 4130 steel used in an airframe critical to the flight-safety was investigated. The tests were performed on hot-rolled steel plate specimens, 0.89 mm thick, with load ratio R = 0.1, constant amplitude, at 20 Hz frequency and room temperature. The results obtained indicated that the axial fatigue strength decreased with the GTAW process itself, and with the subsequent repair cycles, as a consequence of microstructural and microhardness changes and of weld profile geometry factors, which induced high stress concentration at the weld toe.


    Zugriff

    Zugriff über TIB

    Verfügbarkeit in meiner Bibliothek prüfen

    Bestellung bei Subito €


    Exportieren, teilen und zitieren



    Titel :

    Effects of several TIG weld repairs on the axial fatigue strength of AISI 4130 aeronautical steel-welded joints


    Weitere Titelangaben:

    Effekte verschiedener TIG-Schweißreparaturen auf die axiale Ermüdungsfestigkeit von Schweißverbindungen aus AISI 4130 Stahl im Flugzeugbau


    Beteiligte:


    Erscheinungsdatum :

    2012


    Format / Umfang :

    14 Seiten, 15 Bilder, 4 Tabellen, 34 Quellen




    Medientyp :

    Aufsatz (Zeitschrift)


    Format :

    Print


    Sprache :

    Englisch