The application of composites to cryotanks has been one of the major concerns for lightweight launch vehicles. In this study, a prototype of a Type 3 cryotank was fabricated with the composite developed for cryogenic application and aluminum liner, and the cryogenic conditions were applied by filling the prototype with liquid nitrogen and then pressurizing it with gaseous nitrogen. During the experiment, delamination inside the cryotank happened. This article describes several attempts made to investigate failure through both analytical approach with thermo-elastic analysis accompanied by progressive failure and experimental approach with LN2 immersion of composite/aluminum ring specimens.


    Zugriff

    Zugriff über TIB

    Verfügbarkeit in meiner Bibliothek prüfen

    Bestellung bei Subito €


    Exportieren, teilen und zitieren



    Titel :

    Damage analysis of a type 3 cryogenic propellant tank after LN2 storage test


    Weitere Titelangaben:

    Schadensanalyse an einem kryogenen Treibstofftank des Typs 3 nach Speicherung von flüssigem Stickstoff


    Beteiligte:
    Kang, Sang-Guk (Autor:in) / Kim, Myung-Gon (Autor:in) / Park, Sang-Wuk (Autor:in) / Kim, Chun-Gon (Autor:in)

    Erschienen in:

    Erscheinungsdatum :

    2008


    Format / Umfang :

    18 Seiten, 16 Bilder, 3 Tabellen, 34 Quellen




    Medientyp :

    Aufsatz (Zeitschrift)


    Format :

    Print


    Sprache :

    Englisch






    Composite cryogenic propellant tank development

    Robinson, M.J. | Tema Archiv | 1994


    Advanced cryogenic propellant tank development status

    SCHOLZ, E. / LOECHEL, L. / ROBERTS, M. | AIAA | 1992


    Validation of Cryogenic Propellant Tank Self-Pressurization

    Yang, Hong Q. / Patel, Chintan / Williams, Brandon | TIBKAT | 2023