A method for manufacturing a tire member, that improves various performances such as abrasion resistance, tear strength, fatigue resistance and the like of the tire member in good balance is provided. The method includes a step (A) for mixing at least a rubber component, a filler and a thiosulfuric acid compound containing an amino group, and a step (B) for mixing the mixture obtained by the step (A), a sulfur component, and a vulcanization accelerator, wherein the thiosulfuric acid compound containing an amino group is added in an amount of 0.2 parts by mass or more to 100 parts by mass of the rubber component in the step (A), and a temperature of the mixture during mixing is maintained within a range of from 145 to 170° C. for 20 seconds or more in the step (A).


    Zugriff

    Download


    Exportieren, teilen und zitieren



    Titel :

    タイヤ部材及びタイヤの製造方法


    Erscheinungsdatum :

    2016-11-24


    Medientyp :

    Patent


    Format :

    Elektronische Ressource


    Sprache :

    Japanisch


    Klassifikation :

    IPC:    C08J Verarbeitung , WORKING-UP / B60C VEHICLE TYRES , Fahrzeugreifen / C08K Verwendung von anorganischen oder nichtmakromolekularen organischen Stoffen als Zusatzstoffe , USE OF INORGANIC OR NON-MACROMOLECULAR ORGANIC SUBSTANCES AS COMPOUNDING INGREDIENTS / C08L COMPOSITIONS OF MACROMOLECULAR COMPOUNDS , Massen auf Basis makromolekularer Verbindungen